Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % |
Härte, Brinell | 20.0 °C | 179 [-] Show Material materials with Härte, Brinell of 179 [-] |
Yield Strength Rp0.2, short transverse | 20.0 °C | 380 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 380 MPa |
Zugfestigkeit | 20.0 °C | 545 - 760 MPa Show Material materials with Zugfestigkeit of 545 - 760 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.8 - 1.15 % Show Material materials with Chrom of 0.8 - 1.15 % |
Kohlenstoff | 0.35 - 0.5 % Show Material materials with Kohlenstoff of 0.35 - 0.5 % |
Mangan | 0.75 - 1.05 % Show Material materials with Mangan of 0.75 - 1.05 % |
Molybdän | 0.15 - 0.25 % Show Material materials with Molybdän of 0.15 - 0.25 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |