Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 16 % Show Material materials with Dehnung A50 of 16 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 248 [-] Show Material materials with Härte, Brinell of 248 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 690 MPa Show Material materials with Streckgrenze Rp 0,2 of 690 MPa | |
Zugfestigkeit | 23.0 °C | 795 - 965 MPa Show Material materials with Zugfestigkeit of 795 - 965 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 2.3 - 3.3 % Show Material materials with Chrom of 2.3 - 3.3 % |
Kohlenstoff | 0.4 % Show Material materials with Kohlenstoff of 0.4 % |
Mangan | 0.9 % Show Material materials with Mangan of 0.9 % |
Molybdän | 0.8 - 2 % Show Material materials with Molybdän of 0.8 - 2 % |
Nickel | 0.35 % Show Material materials with Nickel of 0.35 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % |
Vanadium | 0.3 - 0.5 % Show Material materials with Vanadium of 0.3 - 0.5 % |