Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Duplex Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 25 % Show Material materials with Dehnung A50 of 25 % | |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | Typical for Duplex Stainless Steel |
Härte, Brinell | 23.0 °C | 293 [-] Show Material materials with Härte, Brinell of 293 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Duplex Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Duplex Stainless Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 MPa | |
Zugfestigkeit | 23.0 °C | 655 MPa Show Material materials with Zugfestigkeit of 655 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 1/K | Typical for Duplex Stainless Steel |
Max. Betriebstemperatur | 300 °C Show Material materials with Max. Betriebstemperatur of 300 °C | Typical for Duplex Stainless Steel | |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 - 502 J/(kg·K) | Typical for Duplex Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 13 - 30 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 - 30 W/(m·K) | Typical for Duplex Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 22 - 23 % Show Material materials with Chrom of 22 - 23 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 0.75 % Show Material materials with Kupfer of 0.75 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 3 - 3.5 % Show Material materials with Molybdän of 3 - 3.5 % |
Nickel | 4.5 - 6.5 % Show Material materials with Nickel of 4.5 - 6.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.14 - 0.2 % Show Material materials with Stickstoff of 0.14 - 0.2 % |