Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 24 % Show Material materials with Dehnung A50 of 24 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Flächenreduzierung | 20.0 °C | 35 % Show Material materials with Flächenreduzierung of 35 % | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Streckgrenze | 20.0 °C | 240 MPa Show Material materials with Streckgrenze of 240 MPa | |
Zugfestigkeit | 20.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel | |
Wärmeleitfähigkeit | 20.0 °C | 34 - 54 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.7 - 0.9 % Show Material materials with Chrom of 0.7 - 0.9 % |
Kohlenstoff | 0.38 - 0.43 % Show Material materials with Kohlenstoff of 0.38 - 0.43 % |
Mangan | 0.6 - 0.9 % Show Material materials with Mangan of 0.6 - 0.9 % |
Molybdän | 0.2 - 0.3 % Show Material materials with Molybdän of 0.2 - 0.3 % |
Nickel | 1.65 - 2 % Show Material materials with Nickel of 1.65 - 2 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 0.3 - 0.6 % Show Material materials with Silizium of 0.3 - 0.6 % |