Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Dichte of 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Ferritic Stainless Steel |
Flächenreduzierung | 23.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % | |
Härte, Brinell | 23.0 °C | 269 [-] Show Material materials with Härte, Brinell of 269 [-] | |
Kerbschlagenergie | 23.0 °C | 40 J Show Material materials with Kerbschlagenergie of 40 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Ferritic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Ferritic Stainless Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 620 MPa Show Material materials with Streckgrenze Rp 0,2 of 620 MPa | |
Zugfestigkeit | 23.0 °C | 760 MPa Show Material materials with Zugfestigkeit of 760 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9.3E-6 - 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Schmelzpunkt | 1425 - 1530 °C Show Material materials with Schmelzpunkt of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 420 - 586 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 22 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.025 % Show Material materials with Aluminium of 0.025 % |
Chrom | 11.5 - 13 % Show Material materials with Chrom of 11.5 - 13 % |
Kohlenstoff | 0.1 - 0.15 % Show Material materials with Kohlenstoff of 0.1 - 0.15 % |
Kupfer | 0.15 % Show Material materials with Kupfer of 0.15 % |
Mangan | 0.25 - 0.8 % Show Material materials with Mangan of 0.25 - 0.8 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 0.75 % Show Material materials with Nickel of 0.75 % |
Niobium | 0.2 % Show Material materials with Niobium of 0.2 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Stickstoff | 0.08 % Show Material materials with Stickstoff of 0.08 % |
Titan | 0.05 % Show Material materials with Titan of 0.05 % |
Wolfram | 0.1 % Show Material materials with Wolfram of 0.1 % |
Zinn | 0.05 % Show Material materials with Zinn of 0.05 % |