Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 13 % Show Material materials with Dehnung A50 of 13 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 30 % Show Material materials with Flächenreduzierung of 30 % | |
Härte, Brinell | 23.0 °C | 331 [-] Show Material materials with Härte, Brinell of 331 [-] | |
Kerbschlagenergie | 23.0 °C | 11 J Show Material materials with Kerbschlagenergie of 11 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 620 MPa Show Material materials with Streckgrenze Rp 0,2 of 620 MPa | |
Zugfestigkeit | 23.0 °C | 965 MPa Show Material materials with Zugfestigkeit of 965 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.025 % Show Material materials with Aluminium of 0.025 % |
Chrom | 11 - 12.5 % Show Material materials with Chrom of 11 - 12.5 % |
Kobalt | 0.2 % Show Material materials with Kobalt of 0.2 % |
Kohlenstoff | 0.2 - 0.25 % Show Material materials with Kohlenstoff of 0.2 - 0.25 % |
Kupfer | 0.15 % Show Material materials with Kupfer of 0.15 % |
Mangan | 0.5 - 1 % Show Material materials with Mangan of 0.5 - 1 % |
Molybdän | 0.9 - 1.25 % Show Material materials with Molybdän of 0.9 - 1.25 % |
Nickel | 0.5 - 1 % Show Material materials with Nickel of 0.5 - 1 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.2 - 0.5 % Show Material materials with Silizium of 0.2 - 0.5 % |
Titan | 0.03 % Show Material materials with Titan of 0.03 % |
Vanadium | 0.2 - 0.3 % Show Material materials with Vanadium of 0.2 - 0.3 % |
Wolfram | 0.9 - 1.25 % Show Material materials with Wolfram of 0.9 - 1.25 % |
Zinn | 0.02 % Show Material materials with Zinn of 0.02 % |