Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % | |
Härte, Brinell | 23.0 °C | 277 [-] Show Material materials with Härte, Brinell of 277 [-] | |
Kerbschlagenergie | 23.0 °C | 27 J Show Material materials with Kerbschlagenergie of 27 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 515 MPa Show Material materials with Streckgrenze Rp 0,2 of 515 MPa | |
Zugfestigkeit | 23.0 °C | 795 MPa Show Material materials with Zugfestigkeit of 795 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Chrom | 11.5 - 13 % Show Material materials with Chrom of 11.5 - 13 % |
Kohlenstoff | 0.13 - 0.18 % Show Material materials with Kohlenstoff of 0.13 - 0.18 % |
Mangan | 0.4 - 0.6 % Show Material materials with Mangan of 0.4 - 0.6 % |
Molybdän | 0.2 % Show Material materials with Molybdän of 0.2 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Niobium | 0.15 - 0.45 % Show Material materials with Niobium of 0.15 - 0.45 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |