Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % |
Flächenreduzierung | 20.0 °C | 45 % Show Material materials with Flächenreduzierung of 45 % |
Härte, Brinell | 20.0 °C | 163 - 217 [-] Show Material materials with Härte, Brinell of 163 - 217 [-] |
Yield Strength Rp0.2, short transverse | 20.0 °C | 310 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 310 MPa |
Zugfestigkeit | 20.0 °C | 550 MPa Show Material materials with Zugfestigkeit of 550 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.2 - 0.35 % Show Material materials with Chrom of 0.2 - 0.35 % |
Kohlenstoff | 0.43 - 0.52 % Show Material materials with Kohlenstoff of 0.43 - 0.52 % |
Mangan | 0.75 - 1.1 % Show Material materials with Mangan of 0.75 - 1.1 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % |
Vanadium | 0.1 % Show Material materials with Vanadium of 0.1 % |