Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % | |
Elastizitätsmodul | 20.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 45 % Show Material materials with Flächenreduzierung of 45 % | |
Härte, Brinell | 20.0 °C | 163 - 217 [-] Show Material materials with Härte, Brinell of 163 - 217 [-] | |
Poissonzahl | 20.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 310 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 310 MPa | |
Zugfestigkeit | 20.0 °C | 550 MPa Show Material materials with Zugfestigkeit of 550 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.8 - 1.2 % Show Material materials with Chrom of 0.8 - 1.2 % |
Kohlenstoff | 0.35 - 0.45 % Show Material materials with Kohlenstoff of 0.35 - 0.45 % |
Mangan | 0.65 - 1 % Show Material materials with Mangan of 0.65 - 1 % |
Molybdän | 0.3 - 0.5 % Show Material materials with Molybdän of 0.3 - 0.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % |
Vanadium | 0.1 % Show Material materials with Vanadium of 0.1 % |