Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 16.5 - 30 % Show Material materials with Dehnung A50 of 16.5 - 30 % |
Streckgrenze | 23.0 °C | 275 MPa Show Material materials with Streckgrenze of 275 MPa |
Zugfestigkeit | 23.0 °C | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.4 % Show Material materials with Chrom of 0.4 % |
Kohlenstoff | 0.35 % Show Material materials with Kohlenstoff of 0.35 % |
Kupfer | 0.4 % Show Material materials with Kupfer of 0.4 % |
Mangan | 0.29 - 1.06 % Show Material materials with Mangan of 0.29 - 1.06 % |
Molybdän | 0.15 % Show Material materials with Molybdän of 0.15 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % |