Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 30 % Show Material materials with Dehnung A50 of 30 % |
Härte, Brinell | 23.0 °C | 179 [-] Show Material materials with Härte, Brinell of 179 [-] |
Härte, Rockwell B | 23.0 °C | 89 [-] Show Material materials with Härte, Rockwell B of 89 [-] |
Streckgrenze | 23.0 °C | 275 MPa Show Material materials with Streckgrenze of 275 MPa |
Zugfestigkeit | 23.0 °C | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.35 % Show Material materials with Kohlenstoff of 0.35 % |
Mangan | 0.29 - 1.06 % Show Material materials with Mangan of 0.29 - 1.06 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |