Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 25 % Show Material materials with Dehnung A50 of 25 % |
Härte, Brinell | 23.0 °C | 170 [-] Show Material materials with Härte, Brinell of 170 [-] |
Härte, Rockwell B | 23.0 °C | 87 [-] Show Material materials with Härte, Rockwell B of 87 [-] |
Streckgrenze | 23.0 °C | 255 MPa Show Material materials with Streckgrenze of 255 MPa |
Zugfestigkeit | 23.0 °C | 415 MPa Show Material materials with Zugfestigkeit of 415 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.24 - 1.31 % Show Material materials with Chrom of 0.24 - 1.31 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Kupfer | 0.2 - 0.6 % Show Material materials with Kupfer of 0.2 - 0.6 % |
Mangan | 0.55 % Show Material materials with Mangan of 0.55 % |
Nickel | 0.2 - 0.7 % Show Material materials with Nickel of 0.2 - 0.7 % |
Phosphor | 0.06 - 0.16 % Show Material materials with Phosphor of 0.06 - 0.16 % |
Schwefel | 0.06 % Show Material materials with Schwefel of 0.06 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |