Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 22 % Show Material materials with Dehnung A50 of 22 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel |
Flächenreduzierung | 20.0 °C | 40 % Show Material materials with Flächenreduzierung of 40 % | |
Härte, Brinell | 20.0 °C | 149 - 207 [-] Show Material materials with Härte, Brinell of 149 - 207 [-] | |
Kerbschlagenergie | 20.0 °C | 41 J Show Material materials with Kerbschlagenergie of 41 J | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel |
Schubmodule | 20.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 290 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 290 MPa | |
Zugfestigkeit | 20.0 °C | 415 MPa Show Material materials with Zugfestigkeit of 415 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Curie-Temperatur | 20.0 °C | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Kohlenstoff | 0.22 % Show Material materials with Kohlenstoff of 0.22 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 1.15 - 1.5 % Show Material materials with Mangan of 1.15 - 1.5 % |
Molybdän | 0.12 % Show Material materials with Molybdän of 0.12 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Niobium | 0.02 % Show Material materials with Niobium of 0.02 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Stickstoff | 0.01 - 0.03 % Show Material materials with Stickstoff of 0.01 - 0.03 % |
Vanadium | 0.04 - 0.11 % Show Material materials with Vanadium of 0.04 - 0.11 % |