Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 190.0 - 210.0 GPa Show Material materials with Elastizitätsmodul of 190.0 - 210.0 GPa | Typical for Steel | |||
Flächenreduzierung | 40.0 % Show Material materials with Flächenreduzierung of 40.0 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Härte, Brinell | 149.0 - 207.0 [-] Show Material materials with Härte, Brinell of 149.0 - 207.0 [-] | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Kerbschlagenergie | 41.0 J Show Material materials with Kerbschlagenergie of 41.0 J | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging | |
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | |||
Zugfestigkeit | 415.0 MPa Show Material materials with Zugfestigkeit of 415.0 MPa | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 1.5 - 2.0 % Show Material materials with Chrom of 1.5 - 2.0 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Kohlenstoff | 0.2 Show Material materials with Kohlenstoff of 0.2 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Kupfer | 0.4 Show Material materials with Kupfer of 0.4 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Mangan | 0.2 - 0.4 % Show Material materials with Mangan of 0.2 - 0.4 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Molybdän | 0.4 - 0.6 % Show Material materials with Molybdän of 0.4 - 0.6 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Nickel | 2.8 - 3.9 % Show Material materials with Nickel of 2.8 - 3.9 % | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Niobium | 0.02 Show Material materials with Niobium of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Phosphor | 0.02 Show Material materials with Phosphor of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Schwefel | 0.02 Show Material materials with Schwefel of 0.02 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Silizium | 0.35 Show Material materials with Silizium of 0.35 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |
Vanadium | 0.05 Show Material materials with Vanadium of 0.05 | Class 1, Annealed, Normalized, Precipitation Hardened, Quenched and Tempered, Normalized and Tempered, Normalized and Precipitation Hardened, or Quenched and Precipitation Hardened | ASTM A707 | Forging |