Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % |
Flächenreduzierung | 23.0 °C | 45 % Show Material materials with Flächenreduzierung of 45 % |
Streckgrenze | 23.0 °C | 415 MPa Show Material materials with Streckgrenze of 415 MPa |
Zugfestigkeit | 23.0 °C | 585 MPa Show Material materials with Zugfestigkeit of 585 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1 - 1.5 % Show Material materials with Chrom of 1 - 1.5 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Mangan | 0.5 - 0.9 % Show Material materials with Mangan of 0.5 - 0.9 % |
Molybdän | 0.9 - 1.2 % Show Material materials with Molybdän of 0.9 - 1.2 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.2 - 0.6 % Show Material materials with Silizium of 0.2 - 0.6 % |
Vanadium | 0.2 - 0.35 % Show Material materials with Vanadium of 0.2 - 0.35 % |