Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Elastizitätsmodul | 20.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 25 % Show Material materials with Flächenreduzierung of 25 % | |
Poissonzahl | 20.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 760 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 760 MPa | |
Zugfestigkeit | 20.0 °C | 965 MPa Show Material materials with Zugfestigkeit of 965 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 0.05 % Show Material materials with Nickel of 0.05 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 1.5 % Show Material materials with Silizium of 1.5 % |