Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 0 - 22 % Show Material materials with Dehnung A50 of 0 - 22 % |
Flächenreduzierung | 20.0 °C | 0 - 40 % Show Material materials with Flächenreduzierung of 0 - 40 % |
Härte, Brinell | 20.0 °C | 0 - 235 [-] Show Material materials with Härte, Brinell of 0 - 235 [-] |
Härte, Rockwell C | 20.0 °C | 0 - 22 [-] Show Material materials with Härte, Rockwell C of 0 - 22 [-] |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 450 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 450 MPa |
Zugfestigkeit | 20.0 °C | 0 - 620 MPa Show Material materials with Zugfestigkeit of 0 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0 - 0.35 % Show Material materials with Chrom of 0 - 0.35 % |
Kohlenstoff | 0 - 0.3 % Show Material materials with Kohlenstoff of 0 - 0.3 % |
Kupfer | 0 - 0.5 % Show Material materials with Kupfer of 0 - 0.5 % |
Mangan | 1 - 1.4 % Show Material materials with Mangan of 1 - 1.4 % |
Molybdän | 0.1 - 0.3 % Show Material materials with Molybdän of 0.1 - 0.3 % |
Nickel | 0 - 0.5 % Show Material materials with Nickel of 0 - 0.5 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.035 % Show Material materials with Schwefel of 0 - 0.035 % |
Silizium | 0 - 0.8 % Show Material materials with Silizium of 0 - 0.8 % |
Vanadium | 0 - 0.03 % Show Material materials with Vanadium of 0 - 0.03 % |
Wolfram | 0 - 0.1 % Show Material materials with Wolfram of 0 - 0.1 % |