Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 14 % Show Material materials with Dehnung A50 of 14 % |
Flächenreduzierung | 20.0 °C | 30 % Show Material materials with Flächenreduzierung of 30 % |
Yield Strength Rp0.2, short transverse | 20.0 °C | 655 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 655 MPa |
Zugfestigkeit | 20.0 °C | 825 MPa Show Material materials with Zugfestigkeit of 825 MPa |
Chemical properties
Property | Value |
---|---|
Bor | 0.4 % Show Material materials with Bor of 0.4 % |
Kohlenstoff | 0.55 % Show Material materials with Kohlenstoff of 0.55 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Mangan | 0.8 - 1.1 % Show Material materials with Mangan of 0.8 - 1.1 % |
Molybdän | 0.2 - 0.3 % Show Material materials with Molybdän of 0.2 - 0.3 % |
Nickel | 0.03 % Show Material materials with Nickel of 0.03 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % |