Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 22 % Show Material materials with Dehnung A50 of 22 % |
Flächenreduzierung | 20.0 °C | 35 % Show Material materials with Flächenreduzierung of 35 % |
Yield Strength Rp0.2, short transverse | 20.0 °C | 365 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 365 MPa |
Zugfestigkeit | 20.0 °C | 585 MPa Show Material materials with Zugfestigkeit of 585 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.35 % Show Material materials with Chrom of 0.35 % |
Kohlenstoff | 0.3 % Show Material materials with Kohlenstoff of 0.3 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 - 1.4 % Show Material materials with Mangan of 1 - 1.4 % |
Molybdän | 0.1 - 0.3 % Show Material materials with Molybdän of 0.1 - 0.3 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Vanadium | 0.03 % Show Material materials with Vanadium of 0.03 % |
Wolfram | 0.1 % Show Material materials with Wolfram of 0.1 % |