Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Kerbschlagenergie | 23.0 °C | 14 J Show Material materials with Kerbschlagenergie of 14 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 590 MPa Show Material materials with Streckgrenze of 590 MPa | |
Zugfestigkeit | 23.0 °C | 760 MPa Show Material materials with Zugfestigkeit of 760 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Chrom | 58 - 62 % Show Material materials with Chrom of 58 - 62 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.3 % Show Material materials with Stickstoff of 0.3 % |
Titan | 0.5 % Show Material materials with Titan of 0.5 % |