Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Streckgrenze | 23.0 °C | 689 MPa Show Material materials with Streckgrenze of 689 MPa | |
Zugfestigkeit | 23.0 °C | 827 MPa Show Material materials with Zugfestigkeit of 827 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 335 - 481 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 335 - 481 J/(kg·K) | Typical for Nickel Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 44 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.15 - 0.25 % Show Material materials with Kohlenstoff of 0.15 - 0.25 % |
Mangan | 0.4 - 0.7 % Show Material materials with Mangan of 0.4 - 0.7 % |
Molybdän | 0.2 - 0.3 % Show Material materials with Molybdän of 0.2 - 0.3 % |
Nickel | 1.65 - 2 % Show Material materials with Nickel of 1.65 - 2 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.045 % Show Material materials with Schwefel of 0.045 % |
Silizium | 0.2 - 0.8 % Show Material materials with Silizium of 0.2 - 0.8 % |