Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Vanadium Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 4 % Show Material materials with Dehnung A50 of 4 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Vanadium Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Vanadium Steel |
Streckgrenze | 23.0 °C | 1172 MPa Show Material materials with Streckgrenze of 1172 MPa | |
Zugfestigkeit | 23.0 °C | 1310 MPa Show Material materials with Zugfestigkeit of 1310 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K | Typical for Chromium Vanadium Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Vanadium Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.8 - 1.1 % Show Material materials with Chrom of 0.8 - 1.1 % |
Kohlenstoff | 0.45 - 0.55 % Show Material materials with Kohlenstoff of 0.45 - 0.55 % |
Mangan | 0.65 - 0.95 % Show Material materials with Mangan of 0.65 - 0.95 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.045 % Show Material materials with Schwefel of 0.045 % |
Silizium | 0.2 - 0.8 % Show Material materials with Silizium of 0.2 - 0.8 % |
Vanadium | 0.15 % Show Material materials with Vanadium of 0.15 % |