Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Dichte of 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Ferritic Stainless Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Ferritic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Ferritic Stainless Steel |
Zugfestigkeit | 23.0 °C | 620 MPa Show Material materials with Zugfestigkeit of 620 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9.3E-6 - 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Schmelzpunkt | 1425 - 1530 °C Show Material materials with Schmelzpunkt of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 420 - 586 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 22 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 17.5 - 19.5 % Show Material materials with Chrom of 17.5 - 19.5 % |
Kohlenstoff | 0.025 % Show Material materials with Kohlenstoff of 0.025 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 1.75 - 2.5 % Show Material materials with Molybdän of 1.75 - 2.5 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Stickstoff | 0.04 % Show Material materials with Stickstoff of 0.04 % |