Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 21 % Show Material materials with Dehnung A50 of 21 % |
Elongation A200 | 23.0 °C | 17 % Show Material materials with Elongation A200 of 17 % |
Streckgrenze | 23.0 °C | 275 MPa Show Material materials with Streckgrenze of 275 MPa |
Zugfestigkeit | 23.0 °C | 485 - 620 MPa Show Material materials with Zugfestigkeit of 485 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.21 % Show Material materials with Kohlenstoff of 0.21 % |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % |
Nickel | 2.1 - 2.5 % Show Material materials with Nickel of 2.1 - 2.5 % |
Phosphor | 0.7 % Show Material materials with Phosphor of 0.7 % |
Schwefel | 0.8 % Show Material materials with Schwefel of 0.8 % |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % |