Mechanisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Streckgrenze | 275 MPa Show Material materials with Streckgrenze of 275 MPa | Normalized | ASTM A203 | Plate |
Zugfestigkeit | 485 - 620 MPa Show Material materials with Zugfestigkeit of 485 - 620 MPa | Normalized | ASTM A203 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % | Normalized | ASTM A203 | Plate |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % | Normalized | ASTM A203 | Plate |
Nickel | 3.25 - 3.75 % Show Material materials with Nickel of 3.25 - 3.75 % | Normalized | ASTM A203 | Plate |
Phosphor | 0.7 % Show Material materials with Phosphor of 0.7 % | Normalized | ASTM A203 | Plate |
Schwefel | 0.8 % Show Material materials with Schwefel of 0.8 % | Normalized | ASTM A203 | Plate |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | Normalized | ASTM A203 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |