Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 16.7 % Show Material materials with Dehnung of 16.7 % | Predicted Value, A200 | |||
19.0 % Show Material materials with Dehnung of 19.0 % | Predicted Value, Transverse | ||||
19.5 % Show Material materials with Dehnung of 19.5 % | Predicted Value, A80 | ||||
20 % Show Material materials with Dehnung of 20 % | Quenched and Tempered | ASTM A203 | Plate | A50 | |
20.8 % Show Material materials with Dehnung of 20.8 % | Predicted Value, A80 Transverse | ||||
21.8 % Show Material materials with Dehnung of 21.8 % | Predicted Value | ||||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel | |||
Flächenreduzierung | 43.1 % Show Material materials with Flächenreduzierung of 43.1 % | Predicted Value | |||
43.6 % Show Material materials with Flächenreduzierung of 43.6 % | Predicted Value, Transverse | ||||
Härte, Brinell | 262 [-] Show Material materials with Härte, Brinell of 262 [-] | Predicted Value, Transverse | |||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel | |||
Scherfestigkeit | 526 MPa Show Material materials with Scherfestigkeit of 526 MPa | Predicted Value | |||
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel | |||
Streckgrenze | 263.2 MPa Show Material materials with Streckgrenze of 263.2 MPa | Predicted Value, RP1 | |||
297.6 MPa Show Material materials with Streckgrenze of 297.6 MPa | Predicted Value, RP05 | ||||
317.5 MPa Show Material materials with Streckgrenze of 317.5 MPa | Predicted Value, RP1 Transverse | ||||
343.2 MPa Show Material materials with Streckgrenze of 343.2 MPa | Predicted Value, Transverse | ||||
345 MPa Show Material materials with Streckgrenze of 345 MPa | Quenched and Tempered | ASTM A203 | Plate | ||
380 MPa Show Material materials with Streckgrenze of 380 MPa | Quenched and Tempered | ASTM A203 | Plate | ||
414.1 MPa Show Material materials with Streckgrenze of 414.1 MPa | Predicted Value, RP02 | ||||
473.4 MPa Show Material materials with Streckgrenze of 473.4 MPa | Predicted Value, RP002 | ||||
475.8 MPa Show Material materials with Streckgrenze of 475.8 MPa | Predicted Value, RP02 Transverse | ||||
Zugfestigkeit | 550 - 690 MPa Show Material materials with Zugfestigkeit of 550 - 690 MPa | Quenched and Tempered | ASTM A203 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 337.4 °C Show Material materials with Max. Betriebstemperatur of 337.4 °C | Predicted Value, Long |
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 7 S/m Show Material materials with Elektrische Leitfähigkeit of 7 S/m | Predicted Value |
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % | Quenched and Tempered | ASTM A203 | Plate |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % | Quenched and Tempered | ASTM A203 | Plate |
Nickel | 3.25 - 3.75 % Show Material materials with Nickel of 3.25 - 3.75 % | Quenched and Tempered | ASTM A203 | Plate |
Phosphor | 0.7 % Show Material materials with Phosphor of 0.7 % | Quenched and Tempered | ASTM A203 | Plate |
Schwefel | 0.8 % Show Material materials with Schwefel of 0.8 % | Quenched and Tempered | ASTM A203 | Plate |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | Quenched and Tempered | ASTM A203 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |