Mechanisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Zugfestigkeit | 450 - 585 MPa Show Material materials with Zugfestigkeit of 450 - 585 MPa | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.18 % Show Material materials with Kohlenstoff of 0.18 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Mangan | 0.9 % Show Material materials with Mangan of 0.9 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Molybdän | 0.45 - 0.6 % Show Material materials with Molybdän of 0.45 - 0.6 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |