Mechanisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Streckgrenze | 345 MPa Show Material materials with Streckgrenze of 345 MPa | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Zugfestigkeit | 550 - 690 MPa Show Material materials with Zugfestigkeit of 550 - 690 MPa | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Mangan | 1.15 - 1.5 % Show Material materials with Mangan of 1.15 - 1.5 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Molybdän | 0.45 - 0.6 % Show Material materials with Molybdän of 0.45 - 0.6 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Nickel | 0.7 - 1 % Show Material materials with Nickel of 0.7 - 1 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |