Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 321 - 363 [-] Show Material materials with Härte, Brinell of 321 - 363 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.06 % Show Material materials with Aluminium of 0.06 % |
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % |
Kohlenstoff | 0.67 - 0.77 % Show Material materials with Kohlenstoff of 0.67 - 0.77 % |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % |
Mangan | 0.6 - 0.9 % Show Material materials with Mangan of 0.6 - 0.9 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.005 - 0.04 % Show Material materials with Schwefel of 0.005 - 0.04 % |
Silizium | 0.15 - 1 % Show Material materials with Silizium of 0.15 - 1 % |
Titan | 0.03 % Show Material materials with Titan of 0.03 % |
Vanadium | 0.06 % Show Material materials with Vanadium of 0.06 % |