Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 14 - 16 % Show Material materials with Dehnung A50 of 14 - 16 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Flächenreduzierung | 23.0 °C | 45 % Show Material materials with Flächenreduzierung of 45 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Chromium Molybdenum Steel |
Schubmodule | 23.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Streckgrenze | 23.0 °C | 620 - 690 MPa Show Material materials with Streckgrenze of 620 - 690 MPa | |
Zugfestigkeit | 23.0 °C | 725 - 930 MPa Show Material materials with Zugfestigkeit of 725 - 930 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Bor | 5E-4 % Show Material materials with Bor of 5E-4 % |
Chrom | 0.4 - 0.65 % Show Material materials with Chrom of 0.4 - 0.65 % |
Kohlenstoff | 0.12 - 0.21 % Show Material materials with Kohlenstoff of 0.12 - 0.21 % |
Mangan | 0.95 - 1.3 % Show Material materials with Mangan of 0.95 - 1.3 % |
Molybdän | 0.2 - 0.3 % Show Material materials with Molybdän of 0.2 - 0.3 % |
Nickel | 0.3 - 0.7 % Show Material materials with Nickel of 0.3 - 0.7 % |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |
Titan | 0.1 % Show Material materials with Titan of 0.1 % |
Vanadium | 0.03 - 0.08 % Show Material materials with Vanadium of 0.03 - 0.08 % |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |