Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 14 - 16 % Show Material materials with Dehnung A50 of 14 - 16 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 45 % Show Material materials with Flächenreduzierung of 45 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 620 - 690 MPa Show Material materials with Streckgrenze of 620 - 690 MPa | |
Zugfestigkeit | 23.0 °C | 725 - 930 MPa Show Material materials with Zugfestigkeit of 725 - 930 MPa |
Chemical properties
Property | Value |
---|---|
Bor | 1E-3 - 5E-3 % Show Material materials with Bor of 1E-3 - 5E-3 % |
Chrom | 0.85 - 1.2 % Show Material materials with Chrom of 0.85 - 1.2 % |
Kohlenstoff | 0.12 - 0.21 % Show Material materials with Kohlenstoff of 0.12 - 0.21 % |
Mangan | 0.45 - 0.7 % Show Material materials with Mangan of 0.45 - 0.7 % |
Molybdän | 0.45 - 0.6 % Show Material materials with Molybdän of 0.45 - 0.6 % |
Nickel | 1.2 - 1.5 % Show Material materials with Nickel of 1.2 - 1.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.2 - 0.35 % Show Material materials with Silizium of 0.2 - 0.35 % |
Titan | 0.1 % Show Material materials with Titan of 0.1 % |