Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 12.0 % Show Material materials with Dehnung of 12.0 % | Predicted Value, A200 | |||
14 % Show Material materials with Dehnung of 14 % | Quenched and Tempered | ASTM A542 | Plate | A50 | |
16.1 % Show Material materials with Dehnung of 16.1 % | Predicted Value, A80 | ||||
18.4 % Show Material materials with Dehnung of 18.4 % | Predicted Value, Transverse | ||||
19.9 % Show Material materials with Dehnung of 19.9 % | Predicted Value | ||||
20.2 % Show Material materials with Dehnung of 20.2 % | Predicted Value, A80 Transverse | ||||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Flächenreduzierung | 42.2 % Show Material materials with Flächenreduzierung of 42.2 % | Predicted Value | |||
45.0 % Show Material materials with Flächenreduzierung of 45.0 % | Predicted Value, Transverse | ||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Scherfestigkeit | 615.8 MPa Show Material materials with Scherfestigkeit of 615.8 MPa | Predicted Value | |||
Schubmodule | 80.0 GPa Show Material materials with Schubmodule of 80.0 GPa | Predicted Value | |||
Streckgrenze | 309 MPa Show Material materials with Streckgrenze of 309 MPa | Predicted Value, RP1 | |||
330.2 MPa Show Material materials with Streckgrenze of 330.2 MPa | Predicted Value, RP1 Transverse | ||||
363.4 MPa Show Material materials with Streckgrenze of 363.4 MPa | Predicted Value, RP05 | ||||
491.2 MPa Show Material materials with Streckgrenze of 491.2 MPa | Predicted Value, RP02 Transverse | ||||
494.5 MPa Show Material materials with Streckgrenze of 494.5 MPa | Predicted Value, Transverse | ||||
585 MPa Show Material materials with Streckgrenze of 585 MPa | Quenched and Tempered | ASTM A542 | Plate | ||
601.8 MPa Show Material materials with Streckgrenze of 601.8 MPa | Predicted Value, RP02 | ||||
643.1 MPa Show Material materials with Streckgrenze of 643.1 MPa | Predicted Value, RP002 | ||||
Zugfestigkeit | 725 - 860 MPa Show Material materials with Zugfestigkeit of 725 - 860 MPa | Quenched and Tempered | ASTM A542 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.1e-05 - 1.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Spezifische Wärmekapazität | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 2 - 2.5 % Show Material materials with Chrom of 2 - 2.5 % | Quenched and Tempered | ASTM A542 | Plate |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % | Quenched and Tempered | ASTM A542 | Plate |
Kupfer | 0.4 % Show Material materials with Kupfer of 0.4 % | Quenched and Tempered | ASTM A542 | Plate |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % | Quenched and Tempered | ASTM A542 | Plate |
Molybdän | 0.9 - 1.1 % Show Material materials with Molybdän of 0.9 - 1.1 % | Quenched and Tempered | ASTM A542 | Plate |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % | Quenched and Tempered | ASTM A542 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | Quenched and Tempered | ASTM A542 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | Quenched and Tempered | ASTM A542 | Plate |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | Quenched and Tempered | ASTM A542 | Plate |
Vanadium | 0.03 % Show Material materials with Vanadium of 0.03 % | Quenched and Tempered | ASTM A542 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |