Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 12.6 % Show Material materials with Dehnung of 12.6 % | Predicted Value, A200 | |||
14 % Show Material materials with Dehnung of 14 % | Quenched and Tempered | ASTM A543 | Plate | A50 | |
17.1 % Show Material materials with Dehnung of 17.1 % | Predicted Value, A80 | ||||
18.4 % Show Material materials with Dehnung of 18.4 % | Predicted Value, Transverse | ||||
20.2 % Show Material materials with Dehnung of 20.2 % | Predicted Value, A80 Transverse | ||||
20.5 % Show Material materials with Dehnung of 20.5 % | Predicted Value | ||||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | |||
Flächenreduzierung | 43.5 % Show Material materials with Flächenreduzierung of 43.5 % | Predicted Value, Transverse | |||
44.8 % Show Material materials with Flächenreduzierung of 44.8 % | Predicted Value | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | |||
Scherfestigkeit | 618.1 MPa Show Material materials with Scherfestigkeit of 618.1 MPa | Predicted Value | |||
Schubmodule | 79.5 GPa Show Material materials with Schubmodule of 79.5 GPa | Predicted Value | |||
Streckgrenze | 318.2 MPa Show Material materials with Streckgrenze of 318.2 MPa | Predicted Value, RP1 | |||
330.7 MPa Show Material materials with Streckgrenze of 330.7 MPa | Predicted Value, RP1 Transverse | ||||
332 MPa Show Material materials with Streckgrenze of 332 MPa | Predicted Value, RP05 | ||||
490 MPa Show Material materials with Streckgrenze of 490 MPa | Predicted Value, RP02 Transverse | ||||
495 MPa Show Material materials with Streckgrenze of 495 MPa | Predicted Value, Transverse | ||||
585 MPa Show Material materials with Streckgrenze of 585 MPa | Quenched and Tempered | ASTM A543 | Plate | ||
596.7 MPa Show Material materials with Streckgrenze of 596.7 MPa | Predicted Value, RP02 | ||||
663.5 MPa Show Material materials with Streckgrenze of 663.5 MPa | Predicted Value, RP002 | ||||
Zugfestigkeit | 725 - 860 MPa Show Material materials with Zugfestigkeit of 725 - 860 MPa | Quenched and Tempered | ASTM A543 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.88 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.88 1/K | Predicted Value |
Spezifische Wärmekapazität | 458.5 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 458.5 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 31.3 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 31.3 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 1 - 1.9 % Show Material materials with Chrom of 1 - 1.9 % | Quenched and Tempered | ASTM A543 | Plate |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % | Quenched and Tempered | ASTM A543 | Plate |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % | Quenched and Tempered | ASTM A543 | Plate |
Molybdän | 0.2 - 0.65 % Show Material materials with Molybdän of 0.2 - 0.65 % | Quenched and Tempered | ASTM A543 | Plate |
Nickel | 2.25 - 4 % Show Material materials with Nickel of 2.25 - 4 % | Quenched and Tempered | ASTM A543 | Plate |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % | Quenched and Tempered | ASTM A543 | Plate |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % | Quenched and Tempered | ASTM A543 | Plate |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % | Quenched and Tempered | ASTM A543 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |