Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 16 % Show Material materials with Dehnung A50 of 16 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Medium Carbon Steel |
Flächenreduzierung | 23.0 °C | 32 % Show Material materials with Flächenreduzierung of 32 % | |
Härte, Brinell | 23.0 °C | 223 - 277 [-] Show Material materials with Härte, Brinell of 223 - 277 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Medium Carbon Steel |
Schubmodule | 23.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Zugfestigkeit | 23.0 °C | 760 MPa Show Material materials with Zugfestigkeit of 760 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.32E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1380 - 1514 °C Show Material materials with Schmelzpunkt of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Spezifische Wärmekapazität | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Wärmeleitfähigkeit | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.06 % Show Material materials with Aluminium of 0.06 % |
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % |
Kohlenstoff | 0.5 - 0.65 % Show Material materials with Kohlenstoff of 0.5 - 0.65 % |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % |
Mangan | 0.6 - 0.9 % Show Material materials with Mangan of 0.6 - 0.9 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.005 - 0.04 % Show Material materials with Schwefel of 0.005 - 0.04 % |
Silizium | 0.15 - 1 % Show Material materials with Silizium of 0.15 - 1 % |
Titan | 0.03 % Show Material materials with Titan of 0.03 % |
Vanadium | 0.04 % Show Material materials with Vanadium of 0.04 % |