Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 16 % Show Material materials with Dehnung of 16 % | Predicted Value, A200 | |||
17.7 % Show Material materials with Dehnung of 17.7 % | Predicted Value, A80 | ||||
18.8 % Show Material materials with Dehnung of 18.8 % | Predicted Value, Transverse | ||||
19.1 % Show Material materials with Dehnung of 19.1 % | Predicted Value, A80 Transverse | ||||
20 % Show Material materials with Dehnung of 20 % | Quenched and Tempered | ASTM A542 | Plate | A50 | |
23.4 % Show Material materials with Dehnung of 23.4 % | Predicted Value | ||||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Flächenreduzierung | 42.5 % Show Material materials with Flächenreduzierung of 42.5 % | Predicted Value, Transverse | |||
46 % Show Material materials with Flächenreduzierung of 46 % | Predicted Value | ||||
Kerbschlagenergie | 54 J Show Material materials with Kerbschlagenergie of 54 J | Quenched and Tempered | ASTM A542 | Plate | |
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Scherfestigkeit | 625.1 MPa Show Material materials with Scherfestigkeit of 625.1 MPa | Predicted Value | |||
Schubmodule | 79.3 GPa Show Material materials with Schubmodule of 79.3 GPa | Predicted Value | |||
Streckgrenze | 299.3 MPa Show Material materials with Streckgrenze of 299.3 MPa | Predicted Value, RP1 | |||
328.6 MPa Show Material materials with Streckgrenze of 328.6 MPa | Predicted Value, RP1 Transverse | ||||
380 MPa Show Material materials with Streckgrenze of 380 MPa | Quenched and Tempered | ASTM A542 | Plate | ||
382.8 MPa Show Material materials with Streckgrenze of 382.8 MPa | Predicted Value, Transverse | ||||
421.1 MPa Show Material materials with Streckgrenze of 421.1 MPa | Predicted Value, RP05 | ||||
432.2 MPa Show Material materials with Streckgrenze of 432.2 MPa | Predicted Value, RP02 | ||||
455.6 MPa Show Material materials with Streckgrenze of 455.6 MPa | Predicted Value, RP02 Transverse | ||||
536.6 MPa Show Material materials with Streckgrenze of 536.6 MPa | Predicted Value, RP002 | ||||
Zugfestigkeit | 585 - 760 MPa Show Material materials with Zugfestigkeit of 585 - 760 MPa | Quenched and Tempered | ASTM A542 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.1e-05 - 1.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Spezifische Wärmekapazität | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 2.75 - 3.25 % Show Material materials with Chrom of 2.75 - 3.25 % | Quenched and Tempered | ASTM A542 | Plate |
Kohlenstoff | 0.1 - 0.15 % Show Material materials with Kohlenstoff of 0.1 - 0.15 % | Quenched and Tempered | ASTM A542 | Plate |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % | Quenched and Tempered | ASTM A542 | Plate |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % | Quenched and Tempered | ASTM A542 | Plate |
Molybdän | 0.9 - 1.1 % Show Material materials with Molybdän of 0.9 - 1.1 % | Quenched and Tempered | ASTM A542 | Plate |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % | Quenched and Tempered | ASTM A542 | Plate |
Niobium | 0.015 - 0.07 % Show Material materials with Niobium of 0.015 - 0.07 % | Quenched and Tempered | ASTM A542 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | Quenched and Tempered | ASTM A542 | Plate |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % | Quenched and Tempered | ASTM A542 | Plate |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % | Quenched and Tempered | ASTM A542 | Plate |
Vanadium | 0.2 - 0.3 % Show Material materials with Vanadium of 0.2 - 0.3 % | Quenched and Tempered | ASTM A542 | Plate |
Technological properties