Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % |
Kerbschlagenergie | 23.0 °C | 27 - 34 J Show Material materials with Kerbschlagenergie of 27 - 34 J |
Streckgrenze Rp 0,2 | 23.0 °C | 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 MPa |
Zugfestigkeit | 23.0 °C | 655 - 795 MPa Show Material materials with Zugfestigkeit of 655 - 795 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 - 0.12 % Show Material materials with Aluminium of 0.02 - 0.12 % |
Kohlenstoff | 0.13 % Show Material materials with Kohlenstoff of 0.13 % |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % |
Molybdän | 0.2 - 0.35 % Show Material materials with Molybdän of 0.2 - 0.35 % |
Nickel | 4.8 - 5.2 % Show Material materials with Nickel of 4.8 - 5.2 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.2 - 0.4 % Show Material materials with Silizium of 0.2 - 0.4 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |