Mechanisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kerbschlagenergie | 27 J Show Material materials with Kerbschlagenergie of 27 J | Heat-Treated | ASTM A738 | Plate |
Streckgrenze | 310 MPa Show Material materials with Streckgrenze of 310 MPa | Heat-Treated | ASTM A738 | Plate |
Zugfestigkeit | 515 - 655 MPa Show Material materials with Zugfestigkeit of 515 - 655 MPa | Heat-Treated | ASTM A738 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | Heat-Treated | ASTM A738 | Plate |
Kohlenstoff | 0.24 % Show Material materials with Kohlenstoff of 0.24 % | Heat-Treated | ASTM A738 | Plate |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % | Heat-Treated | ASTM A738 | Plate |
Molybdän | 0.08 % Show Material materials with Molybdän of 0.08 % | Heat-Treated | ASTM A738 | Plate |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | Heat-Treated | ASTM A738 | Plate |
Niobium | 0.04 % Show Material materials with Niobium of 0.04 % | Heat-Treated | ASTM A738 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Silizium | 0.15 - 0.5 % Show Material materials with Silizium of 0.15 - 0.5 % | Heat-Treated | ASTM A738 | Plate |
Vanadium | 0.07 % Show Material materials with Vanadium of 0.07 % | Heat-Treated | ASTM A738 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |