Mechanisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kerbschlagenergie | 27 J Show Material materials with Kerbschlagenergie of 27 J | Heat-Treated | ASTM A738 | Plate |
Streckgrenze | 315 MPa Show Material materials with Streckgrenze of 315 MPa | Heat-Treated | ASTM A738 | Plate |
380 MPa Show Material materials with Streckgrenze of 380 MPa | Heat-Treated | ASTM A738 | Plate | |
415 MPa Show Material materials with Streckgrenze of 415 MPa | Heat-Treated | ASTM A738 | Plate | |
Zugfestigkeit | 485 - 620 MPa Show Material materials with Zugfestigkeit of 485 - 620 MPa | Heat-Treated | ASTM A738 | Plate |
515 - 655 MPa Show Material materials with Zugfestigkeit of 515 - 655 MPa | Heat-Treated | ASTM A738 | Plate | |
550 - 690 MPa Show Material materials with Zugfestigkeit of 550 - 690 MPa | Heat-Treated | ASTM A738 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | Heat-Treated | ASTM A738 | Plate |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % | Heat-Treated | ASTM A738 | Plate |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % | Heat-Treated | ASTM A738 | Plate |
Molybdän | 0.08 % Show Material materials with Molybdän of 0.08 % | Heat-Treated | ASTM A738 | Plate |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | Heat-Treated | ASTM A738 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Silizium | 0.15 - 0.5 % Show Material materials with Silizium of 0.15 - 0.5 % | Heat-Treated | ASTM A738 | Plate |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % | Heat-Treated | ASTM A738 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |