Mechanisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kerbschlagenergie | 27 J Show Material materials with Kerbschlagenergie of 27 J | Heat-Treated | ASTM A738 | Plate |
Streckgrenze | 515 MPa Show Material materials with Streckgrenze of 515 MPa | Heat-Treated | ASTM A738 | Plate |
Zugfestigkeit | 620 - 760 MPa Show Material materials with Zugfestigkeit of 620 - 760 MPa | Heat-Treated | ASTM A738 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | Heat-Treated | ASTM A738 | Plate |
Bor | 0.0007 % Show Material materials with Bor of 0.0007 % | Heat-Treated | ASTM A738 | Plate |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % | Heat-Treated | ASTM A738 | Plate |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % | Heat-Treated | ASTM A738 | Plate |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Mangan | 1.1 - 1.6 % Show Material materials with Mangan of 1.1 - 1.6 % | Heat-Treated | ASTM A738 | Plate |
Molybdän | 0.35 % Show Material materials with Molybdän of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Nickel | 0.7 % Show Material materials with Nickel of 0.7 % | Heat-Treated | ASTM A738 | Plate |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | Heat-Treated | ASTM A738 | Plate |
Phosphor | 0.015 % Show Material materials with Phosphor of 0.015 % | Heat-Treated | ASTM A738 | Plate |
Schwefel | 0.006 % Show Material materials with Schwefel of 0.006 % | Heat-Treated | ASTM A738 | Plate |
Silizium | 0.15 - 0.5 % Show Material materials with Silizium of 0.15 - 0.5 % | Heat-Treated | ASTM A738 | Plate |
Vanadium | 0.09 % Show Material materials with Vanadium of 0.09 % | Heat-Treated | ASTM A738 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |