Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 14.2 % Show Material materials with Dehnung of 14.2 % | Predicted Value, A200 |
15.6 % Show Material materials with Dehnung of 15.6 % | Predicted Value, A80 | |
18.3 % Show Material materials with Dehnung of 18.3 % | Predicted Value, Transverse | |
19.6 % Show Material materials with Dehnung of 19.6 % | Predicted Value, A80 Transverse | |
20.3 % Show Material materials with Dehnung of 20.3 % | Predicted Value, A5 | |
21.2 % Show Material materials with Dehnung of 21.2 % | Predicted Value, A50 | |
21.4 % Show Material materials with Dehnung of 21.4 % | Predicted Value | |
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 41.6 % Show Material materials with Flächenreduzierung of 41.6 % | Predicted Value |
43.1 % Show Material materials with Flächenreduzierung of 43.1 % | Predicted Value, Transverse | |
Härte, Brinell | 244 [-] Show Material materials with Härte, Brinell of 244 [-] | Predicted Value, Transverse |
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Scherfestigkeit | 515.9 MPa Show Material materials with Scherfestigkeit of 515.9 MPa | Predicted Value |
Schubmodule | 79.5 GPa Show Material materials with Schubmodule of 79.5 GPa | Predicted Value |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.78 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.78 1/K | Predicted Value |
Max. Betriebstemperatur | 299.5 °C Show Material materials with Max. Betriebstemperatur of 299.5 °C | Predicted Value, Long |
Spezifische Wärmekapazität | 460.9 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460.9 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 40.51 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 40.51 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Related Standards |
---|---|---|
Kohlenstoff | 0.23 % Show Material materials with Kohlenstoff of 0.23 % | ASTM A572 |
Mangan | 1.65 % Show Material materials with Mangan of 1.65 % | ASTM A572 |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | ASTM A572 |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | ASTM A572 |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | ASTM A572 |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |