Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 17.5 % Show Material materials with Dehnung of 17.5 % | Predicted Value, A80 | |||
18 % Show Material materials with Dehnung of 18 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | A200 | |
19.4 % Show Material materials with Dehnung of 19.4 % | Predicted Value, Transverse | ||||
20.0 % Show Material materials with Dehnung of 20.0 % | Predicted Value, A80 Transverse | ||||
22 % Show Material materials with Dehnung of 22 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | A50 | |
24.7 % Show Material materials with Dehnung of 24.7 % | Predicted Value | ||||
Elastizitätsmodul | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel | |||
Flächenreduzierung | 39.7 % Show Material materials with Flächenreduzierung of 39.7 % | Predicted Value | |||
43.5 % Show Material materials with Flächenreduzierung of 43.5 % | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel | |||
Scherfestigkeit | 516.5 MPa Show Material materials with Scherfestigkeit of 516.5 MPa | Predicted Value | |||
Schubmodule | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel | |||
Streckgrenze | 266.6 MPa Show Material materials with Streckgrenze of 266.6 MPa | Predicted Value, RP1 | |||
310 MPa Show Material materials with Streckgrenze of 310 MPa | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | ||
316.7 MPa Show Material materials with Streckgrenze of 316.7 MPa | Predicted Value, RP1 Transverse | ||||
345 MPa Show Material materials with Streckgrenze of 345 MPa | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | ||
353.7 MPa Show Material materials with Streckgrenze of 353.7 MPa | Predicted Value, Transverse | ||||
370.7 MPa Show Material materials with Streckgrenze of 370.7 MPa | Predicted Value, RP05 | ||||
371.3 MPa Show Material materials with Streckgrenze of 371.3 MPa | Predicted Value, RP02 | ||||
405.4 MPa Show Material materials with Streckgrenze of 405.4 MPa | Predicted Value, RP002 | ||||
454 MPa Show Material materials with Streckgrenze of 454 MPa | Predicted Value, RP02 Transverse | ||||
Zugfestigkeit | 450 - 585 MPa Show Material materials with Zugfestigkeit of 450 - 585 MPa | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate | |
485 - 620 MPa Show Material materials with Zugfestigkeit of 485 - 620 MPa | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1e-05 - 1.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1e-05 - 1.5e-05 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1370 - 1530 °C Show Material materials with Schmelzpunkt of 1370 - 1530 °C | Typical for Martensitic Stainless Steel |
Spezifische Wärmekapazität | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Mangan | 0.7 - 1.35 % Show Material materials with Mangan of 0.7 - 1.35 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Molybdän | 0.08 % Show Material materials with Molybdän of 0.08 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Niobium | 0.03 % Show Material materials with Niobium of 0.03 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Silizium | 0.15 - 0.5 % Show Material materials with Silizium of 0.15 - 0.5 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Vanadium | 0.06 % Show Material materials with Vanadium of 0.06 % | Thermo-Mechanical Control Process (TMCP) | ASTM A841 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |