Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 14 % Show Material materials with Dehnung A50 of 14 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 40 % Show Material materials with Flächenreduzierung of 40 % | |
Kerbschlagenergie | 23.0 °C | 41 J Show Material materials with Kerbschlagenergie of 41 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Yield strength Rp0.02 | 23.0 °C | 860 MPa Show Material materials with Yield strength Rp0.02 of 860 MPa | |
Zugfestigkeit | 23.0 °C | 965 MPa Show Material materials with Zugfestigkeit of 965 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.7 - 1.25 % Show Material materials with Chrom of 0.7 - 1.25 % |
Kohlenstoff | 0.45 % Show Material materials with Kohlenstoff of 0.45 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 0.2 % Show Material materials with Molybdän of 0.2 % |
Nickel | 1.65 - 3.5 % Show Material materials with Nickel of 1.65 - 3.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |
Vanadium | 0.07 - 0.12 % Show Material materials with Vanadium of 0.07 - 0.12 % |