Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 25 - 28 % Show Material materials with Dehnung A50 of 25 - 28 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 60 % Show Material materials with Flächenreduzierung of 60 % | |
Kerbschlagenergie | 23.0 °C | 95 J Show Material materials with Kerbschlagenergie of 95 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 760 - 930 MPa Show Material materials with Streckgrenze Rp 0,2 of 760 - 930 MPa | |
Zugfestigkeit | 23.0 °C | 830 - 1000 MPa Show Material materials with Zugfestigkeit of 830 - 1000 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.04 % Show Material materials with Aluminium of 0.04 % |
Chrom | 17.5 - 20 % Show Material materials with Chrom of 17.5 - 20 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 17.5 - 20 % Show Material materials with Mangan of 17.5 - 20 % |
Nickel | 2 % Show Material materials with Nickel of 2 % |
Phosphor | 0.06 % Show Material materials with Phosphor of 0.06 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |
Stickstoff | 0.45 - 0.8 % Show Material materials with Stickstoff of 0.45 - 0.8 % |
Titan | 0.1 % Show Material materials with Titan of 0.1 % |
Vanadium | 0.25 % Show Material materials with Vanadium of 0.25 % |