Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Steel |
Härte, Brinell | 20.0 °C | 207 [-] Show Material materials with Härte, Brinell of 207 [-] | |
Härte, Rockwell B | 20.0 °C | 92 [-] Show Material materials with Härte, Rockwell B of 92 [-] | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 9.4E-6 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.4E-6 - 1.5E-5 1/K | Typical for Chromium Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Steel | |
Spezifische Wärmekapazität | 20.0 °C | 440 - 494 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
Wärmeleitfähigkeit | 20.0 °C | 23 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 23 - 50 W/(m·K) | Typical for Chromium Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Chrom | 1.35 - 1.6 % Show Material materials with Chrom of 1.35 - 1.6 % |
Kohlenstoff | 0.93 - 1.05 % Show Material materials with Kohlenstoff of 0.93 - 1.05 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.25 - 0.45 % Show Material materials with Mangan of 0.25 - 0.45 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Sauerstoff | 1.5E-3 % Show Material materials with Sauerstoff of 1.5E-3 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |