Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Flächenreduzierung | 23.0 °C | 40 % Show Material materials with Flächenreduzierung of 40 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel |
Streckgrenze | 23.0 °C | 415 MPa Show Material materials with Streckgrenze of 415 MPa | |
Zugfestigkeit | 23.0 °C | 620 - 760 MPa Show Material materials with Zugfestigkeit of 620 - 760 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1370 - 1530 °C Show Material materials with Schmelzpunkt of 1370 - 1530 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Antimon | 3E-3 % Show Material materials with Antimon of 3E-3 % |
Arsen | 0.01 % Show Material materials with Arsen of 0.01 % |
Bor | 1E-3 % Show Material materials with Bor of 1E-3 % |
Chrom | 8 - 9.5 % Show Material materials with Chrom of 8 - 9.5 % |
Kohlenstoff | 0.08 - 0.12 % Show Material materials with Kohlenstoff of 0.08 - 0.12 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Mangan | 0.3 - 0.5 % Show Material materials with Mangan of 0.3 - 0.5 % |
Molybdän | 0.85 - 1.05 % Show Material materials with Molybdän of 0.85 - 1.05 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Niobium | 0.06 - 0.1 % Show Material materials with Niobium of 0.06 - 0.1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 5E-3 % Show Material materials with Schwefel of 5E-3 % |
Silizium | 0.2 - 0.4 % Show Material materials with Silizium of 0.2 - 0.4 % |
Stickstoff | 0.04 - 0.07 % Show Material materials with Stickstoff of 0.04 - 0.07 % |
Titan | 0.01 % Show Material materials with Titan of 0.01 % |
Vanadium | 0.18 - 0.25 % Show Material materials with Vanadium of 0.18 - 0.25 % |
Wolfram | 0.05 % Show Material materials with Wolfram of 0.05 % |
Zinn | 0.01 % Show Material materials with Zinn of 0.01 % |
Zirkonium | 0.01 % Show Material materials with Zirkonium of 0.01 % |