Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 223 - 269 [-] Show Material materials with Härte, Brinell of 223 - 269 [-] | |
Härte, Rockwell B | 23.0 °C | 98 - 104 [-] Show Material materials with Härte, Rockwell B of 98 - 104 [-] | |
Härte, Rockwell C | 23.0 °C | 19 - 28 [-] Show Material materials with Härte, Rockwell C of 19 - 28 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.95 - 1.3 % Show Material materials with Aluminium of 0.95 - 1.3 % |
Chrom | 1 - 1.35 % Show Material materials with Chrom of 1 - 1.35 % |
Kohlenstoff | 0.22 - 0.27 % Show Material materials with Kohlenstoff of 0.22 - 0.27 % |
Mangan | 0.5 - 0.7 % Show Material materials with Mangan of 0.5 - 0.7 % |
Molybdän | 0.2 - 0.3 % Show Material materials with Molybdän of 0.2 - 0.3 % |
Nickel | 3.25 - 3.75 % Show Material materials with Nickel of 3.25 - 3.75 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |