Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 17 % Show Material materials with Dehnung A50 of 17 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 45 % Show Material materials with Flächenreduzierung of 45 % | |
Kerbschlagenergie | 23.0 °C | 34 J Show Material materials with Kerbschlagenergie of 34 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Yield strength Rp0.02 | 23.0 °C | 550 MPa Show Material materials with Yield strength Rp0.02 of 550 MPa | |
Zugfestigkeit | 23.0 °C | 690 MPa Show Material materials with Zugfestigkeit of 690 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.5 % Show Material materials with Chrom of 0.5 % |
Kohlenstoff | 0.27 % Show Material materials with Kohlenstoff of 0.27 % |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % |
Molybdän | 0.2 - 0.6 % Show Material materials with Molybdän of 0.2 - 0.6 % |
Nickel | 3 % Show Material materials with Nickel of 3 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Vanadium | 0.03 % Show Material materials with Vanadium of 0.03 % |