Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % |
Flächenreduzierung | 23.0 °C | 38 % Show Material materials with Flächenreduzierung of 38 % |
Streckgrenze Rp 0,2 | 23.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa |
Zugfestigkeit | 23.0 °C | 485 - 655 MPa Show Material materials with Zugfestigkeit of 485 - 655 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.03 % Show Material materials with Aluminium of 0.03 % |
Bor | 3E-3 % Show Material materials with Bor of 3E-3 % |
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % |
Kalzium | 0.02 % Show Material materials with Kalzium of 0.02 % |
Kohlenstoff | 0.35 % Show Material materials with Kohlenstoff of 0.35 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.4 - 1.05 % Show Material materials with Mangan of 0.4 - 1.05 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Niobium | 0.01 % Show Material materials with Niobium of 0.01 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Titan | 0.02 % Show Material materials with Titan of 0.02 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |