Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % |
Flächenreduzierung | 20.0 °C | 38 % Show Material materials with Flächenreduzierung of 38 % |
Yield Strength Rp0.2, short transverse | 20.0 °C | 345 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 345 MPa |
Zugfestigkeit | 20.0 °C | 550 - 725 MPa Show Material materials with Zugfestigkeit of 550 - 725 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.03 % Show Material materials with Aluminium of 0.03 % |
Bor | 3E-3 % Show Material materials with Bor of 3E-3 % |
Chrom | 0.25 - 0.45 % Show Material materials with Chrom of 0.25 - 0.45 % |
Kalzium | 0.02 % Show Material materials with Kalzium of 0.02 % |
Kohlenstoff | 0.27 % Show Material materials with Kohlenstoff of 0.27 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.5 - 1 % Show Material materials with Mangan of 0.5 - 1 % |
Molybdän | 0.55 - 0.7 % Show Material materials with Molybdän of 0.55 - 0.7 % |
Nickel | 0.5 - 1 % Show Material materials with Nickel of 0.5 - 1 % |
Niobium | 0.01 % Show Material materials with Niobium of 0.01 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Titan | 0.02 % Show Material materials with Titan of 0.02 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |