Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 0 - 20 % Show Material materials with Dehnung A50 of 0 - 20 % |
Flächenreduzierung | 20.0 °C | 0 - 48 % Show Material materials with Flächenreduzierung of 0 - 48 % |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 485 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 485 MPa |
Zugfestigkeit | 20.0 °C | 620 - 795 MPa Show Material materials with Zugfestigkeit of 620 - 795 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.03 % Show Material materials with Aluminium of 0 - 0.03 % |
Bor | 0 - 3E-3 % Show Material materials with Bor of 0 - 3E-3 % |
Chrom | 2 - 2.5 % Show Material materials with Chrom of 2 - 2.5 % |
Kalzium | 0 - 0.02 % Show Material materials with Kalzium of 0 - 0.02 % |
Kohlenstoff | 0.11 - 0.15 % Show Material materials with Kohlenstoff of 0.11 - 0.15 % |
Kupfer | 0 - 0.25 % Show Material materials with Kupfer of 0 - 0.25 % |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % |
Molybdän | 0.9 - 1.1 % Show Material materials with Molybdän of 0.9 - 1.1 % |
Nickel | 0 - 0.25 % Show Material materials with Nickel of 0 - 0.25 % |
Niobium | 0 - 0.01 % Show Material materials with Niobium of 0 - 0.01 % |
Phosphor | 0 - 0.02 % Show Material materials with Phosphor of 0 - 0.02 % |
Schwefel | 0 - 0.015 % Show Material materials with Schwefel of 0 - 0.015 % |
Silizium | 0 - 0.35 % Show Material materials with Silizium of 0 - 0.35 % |
Titan | 0 - 0.02 % Show Material materials with Titan of 0 - 0.02 % |
Vanadium | 0 - 0.02 % Show Material materials with Vanadium of 0 - 0.02 % |